News

Why Is The Bearing Roller Quenching? What Is Quenching Soft Spots?

Oct 14, 2022 Leave a message

The bearing manufacturer knows that after quenching, the common quality problems are quenching soft spots. Why is the bearing roller quenching soft dots? What is quenching soft spots?

What is quenching soft spots?


After quenching soft dots, the phenomenon of low hardness after quenching. Due to low hardness, softness will directly affect the quality of grinding processing. During use, fatigue damage will also occur. Avoid the emergence of soft points in production.


There are two main types of quenching soft points, one is decarburized: if the atmosphere in the furnace is not good when heating or heating in the air furnace, it is easy to cause decarbon; Inadequate, so that the substrate is not sufficiently macro -ainerized. After quenching, it cannot be transformed into a genetic tissue. The large amount of methanol is directly dripped on the surface of the workpiece, or the place where the workpiece and workpiece are closely contacted can cause the critical cold speed, and cannot be transformed into martarinosteen tissue.


What are the reasons why the bearing roller quenching the soft point?


1. Analysis of macro -appearance observation and soft dot proportion


After the normal roller quenching through the cold acid, the surface of the roller should be uniformly consistent light gray; and the roller that is quenching the soft dot is washed through cold acid, and the surface of the roller surface is partial Located on the rolling surface.


2. The reason for the soft point of the bearing roller quenching


Through the macro appearance observation, chemical composition analysis, hardness testing and gold phase test analysis of normal roller and soft dot rollers, we can see that the surface of the soft dot roller's gold phase tissue In vitro, there are also needle -shaped and small pieces, and the hardness is significantly lower than the normal roller, and the hardness distribution is uneven. The main reason for the tissue and hardness of the roller rolling surface may be that the cooling speed of the rolling surface during the quenching process may be slower. The over -cold Octoba of the rolling surface during the quenching process has not completely transformed Needle -shaped or block -shaped flexion tissue, so it forms soft spots after quenching.


By increasing the heating temperature, increasing the heat preservation time, and adjusting the parameters that affect the cooling, increase the stirring speed and the speed of moving, the soft dot of the roller Qu's body will still appear. Note. According to the analysis, the rolling surface of the bearing roller cooled during the quenching process. The slower reason may be that the rolling surface of the two rollers when the roller quenchs contacts each other, so that the liquidity of the quenching salt of the rolling surface is relatively poor. The heat generated during the quenching process is quickly taken away, which causes the cooling speed of the rolling surface to contact the area to slow down and the soft spots of quenching.


The reason for the soft point of the roller quenching Qu's body is that during the quenching process, due to the mutual contact between the rolling surface of the roller, the beef is formed. In the actual roller heat treatment process, in order to avoid the soft spots of the roller, the roller should be evenly placed in the disk, and it is strictly forbidden to contact each other between the rolling surfaces.


Send Inquiry